I been insuring my artist studio for over 25 years without a problem. If they need another modifier, use glass: "glass artist studio." It is succinct and accurate.

I was told from the start to avoid terms that stress the industrial aspects of the studio. Thousands of degree...no. Glory hole, no,no. Bushy reducing flame no way. Flame, even worse. And don't invite the agent over when 3 of your best buddies are pulling cane.

After a couple of years without claims they may be more understanding.My agent is happy: I've made no claims. I'd say knock on wood, but there is not much wood in the studio.
__________________
You have to dance with the glass