I have a set of 11ga Kanthal a-1 that are now 18months old, melting cullett, only going to 2150f, very low watt density, fired with a Phase angle S.C.R.

The phase angle fired unit is not the best choice, a burst fired unit would be better.

The info about 2400f is what Tom Littleton put out for just the scenario that you described Brice, Invested pot and gas burner system.

Electric freestanding pots are different.