Oh - and 2400... it's doable. I had mine up to 2400 on the first set of elements (for 10 hours!). It does glow like the sun at that temp, but you must watch the expansion of the glass at those temps. I didn't, and my pot overflowed, prompting the rebuild.

-Richard