Randy, I would guess that they are mounted horizantaly, for just that reason.

All: Since Annealer design is fresh in my mind, and my EXTRA GOOD GAS Handouts are filed in a pile, Is there a Watts per Cu ft figure for the Thumbesque melters? And do you include the pot and glass area in that figure?

Just to throw something back in trade for the expected return.

I'm told annealers ( Blown work) need to be around 500 watts per cu ft, for good heat response. Casting ovens up to a blazing 1000 watts per cu ft. 650, for a decent combo.

Thanks for the info folks

Greg