View Single Post
#
19
03-05-2006, 12:55 AM
Peet Robison
Guest
Posts: n/a
It would make sense to add Potassium Dichromate as that would add oxygen to the melt. Cobalt carb would help also. My point was Manganese alone in cullet would be very difficult to make a dark purple since it needs oxygen.
Peet Robison