View Single Post
  #8  
Old 06-11-2019, 07:38 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,967
Pete VanderLaan is on a distinguished road
not immediately since it would prevent other tests from occurring if it fails.

I would like to see a chemical analysis of both the crucible as well as the interface between the crucible and any glass placed in it since there is a residue. Also testing for just basic failure running the pot up in themperature to see if sintering affects it.

It didn't crack when taken from the gloryhole and put on the marver. It was hot. I think our interest in it is as a form for casting. Corning's might well be something else.

How's the judgement doing.
__________________
Where are we going and why am I in this basket?
Reply With Quote