Take a base mix at 2%. Isolate 5-10 lbs of it and add the additional 2%.

melt that . Fine it. Test it the next day against the clear. Do a ring test at the minimum. I realize I'm asking you to put three days in this but breaking it up is way worse.

This really takes patience to get it right. Most shops refuse to be patient. Respecting process pays off.