Josh Simpson gets all of his purple color from manganese in 4C so I am quite sure it works fine. I did some work on that color for him in January so I know what's in the cullet additive. It has lots and lots of manganese and I melted it in the 4C. Any other suggestions will be greatly appreciated.
|