try upwards of $100 lb . At this point QC is not good but the demand for the colors supersedes the quality issues. If this was soft glass people would be howling/ That 40lb pot costs 165 dollars. The pyrex cullet is expensive.

And Yes Mark doesn't get rid of anything. He used the corhart pots for all the recent experiments for the titanium Phosphate. Scott told me when he was in Murano, he was on melt 161.