Have you found my long description of what I do in the archives?
On a new- graphite- mold it is enough with two layers - it will last several hundred pieces, say on a wineglass cup, on a more complicated mold with sharp edges maybe 50 to a 100- it depends- is it clear glass? Or color on the outside- which is abrasive
I don't have much experience with steel molds, but I imagine its about the same as graphite
i have no experience with 40/80 grit cork- Im in sweden and get the cork from Essemce, and do it like I've said, because thats the way we do it, and it works.