Thanks Pete. This is one job that I never anticipated was possible. Maybe because of the small cavity I have to work in. The pics does not make it easier because they fool you. I realized that a picture is a useful tool is examining the inside of the furnace. I am able to see it from a different angle and am able to see some parts that were not possible from outside. The elements are resting on a grove but it looks like its on the edge.
Now that you can see it. How about if I heat it and cut it then pull them together and twist. Or just heat the excess and twist it?