I sat with Fritz and Kent Ipsen a few years back at VCU and got s-faced on some good whiskey and listened to them tell stories and wishing I had a tape recorder. The old timers aren't going to be around forever and it would be really nice to have a record (even anecdotal) of what happened in the early days, like when did Kugler arrive, who brought it in and who really did throw the trout into the Penland furnace....
|