Quote:
Originally Posted by Pete VanderLaan
***************
When EZ Therm built their shortlived moly, a cooperative adventure between Henry Halem and Mark Jesson from Duralite, they asked Miller for a welder that would perform continuous duty. Miller said "sure" and supplied them with a unit that supplied continuous duty- for an eight hour work shift. This was an exceptionally unfortunate miscalculation and speaks volumes for testing a product for a year before it gets put on the market. It was only one of many problems.
Use a transformer, a real one.
|
Yup. Even the user guide shows 100% duty cycle is actually 8 hours instead of 24 as most would assume. Specsmanship at it's best.