We also revere the Italian masters... Lino comes to mind, but is that because of their glass mixing abilities or their creative object making? Do the Italian masters even know how to make their own glass? Many people want to have all the skills and some want to concentrate on a particular skill. It does not make one person better than another.

I can admire someone’s knowledge of material like Pete’s. I can also admire someone’s blowing skill like David’s. Knowing less about one step of the process doesn’t limit my admiration.

Good thing we all find different things interesting or it would be a boring world.