Originally posted by Dave Bross


Which reminds me....anyone know where to get powder blue in small quantities? [/b]
Make your powder blue. Take 10 grams of cobalt and put it in 90 grams of your mixed batch and stir well. Then when you want a one gram cobalt glass take ten grams of the powder blue instead. Or, mix it the way you like it.