Batch is starting to sound more and more appealing. I look forward to a thread announcement that the East Bay "Vanderlaan" batch is ready for order. Rather than starting with SP87, I think I'll await this version to make the switch. I am loving my chalcedony and look forward to seeing the results with a base glass Pete said would match it very well.
Thanks to Richard for mentioning his positive experience with it as well. I believe our furnace designs are from a similar vein.
I just expanded my own furnace to include two 17 lb color pots. Wow...I could start making some pure opal colors in addition to my cullet based formulas. I wouldn't even be thinking of this if it were not for this forum.
|