I think Dave Bross mentioned here somewhere that strontium and barium were very similar on expansion factor. So I've been entering the strontium in the barium line of the spreadsheet. How accurate that is, I'm not sure yet but is what I've been doing on the spreadsheet for these phosphates I'm doing now which have a decent amt. of strontium.