Quote:
Originally Posted by Pete VanderLaan View Post
The SP chips were totally fined out as a product which made melting in the studio a total dream.

Maybe the ones you got were but, the ones that I have received
(especially lately) still need to be fined out. There are bubbles noticeable in the chips right out of the bag. I like Spruce Pine to work with but, the chips need some work. Like many have said, there is no free lunch. I hope the new method of production for SP chips will be good for us end users.