I wouldn’t want any latex tubing with less then a 1/4” ID and a 1/16” wall.
6mm ID and 1.6mm wall thickness for our fractionaly challenged friends.

Anything smaller makes you work harder blowing and anything thinner kinks at the most inopportune moment. This my personal observation I know some might disagree.