That’s true, and I do love copper blues, but I’m going to be using sulfur in the traditional way anyhow, so why not try (in the quest for knowledge and understanding and such). Also supposedly the blue comes from elemental sulfur which doesn’t stink, only it’s compounds do, so theoretically this sulfur blue wouldn’t smell either. But not having done it yet, I don’t know. I’ll post results, good, bad or indifferent just in case anyone else is interested.
|