Jim dropped the ball and went off to Murano. I don't know if he has come back yet. We have certainly agreed he can mix it. I'll write him again.

If your clear was decolorized with selenium, it's possible you could get a yellow tone. I remember Spruce Pine inadvertently getting a pink at one point that was attributable to Se. Just not a yellow. The Goddess Selen is an interesting woman. I just can't see using cerium for that. Any Cristalica I have from when I brought the stuff over here from Dobern two- three years back for Spruce Pine ( Jeez time flies) showed no color at all. It was water white.