well, I thought that I had gotten all the lead or you wouldn't have any.

Are you planning to case the neo in clear? If so, do a small melt using the basic 2% and add another 2% to that, melt it and try it. If you don't do that, mix a full load and try it and if it doesn't work out, mix that with some straight clear.

I've often felt that the Neo was also a fining agent that was really effective. That interior electron ring does some unpredictable stuff. That color maintains a clarity that I love.

The potassium hydroxide was well stored and seemed clean. It's really handy if you are making silver or copper bases and don't want the oxygen from the carbonate.