Quote:
Originally Posted by Pete VanderLaan
solid castings should be treated with respect and go thru inversion with at least a wink and nod to expansion. Otherwise, it doesn't matter much. With the pot in, you need to behave.
|
The only casting is my rammable gathering port in the maintenance lid. It's removable so I can do that for the test. I'll probably just set the lids on rather than connect up all the hinges until it's working properly.