Quote:
Originally Posted by Rollin Karg View Post
Were going to add another step and start doing as Pete says and leave the door open for 45 seconds after throwing in the batch.
**************
Steve Smyers used to charge charge batches like cad sels and would just shut the furnace off until it glazed over. I think with an electric it would lose a lot of ground doing that but I will throw it out there as an option.

What I notice with those glasses is that the real action doesn't start for about 1.5 hours. At that point it's really smoking. I always throw in all of the batch in one charge. I don't like multiple charges on Cad Sel stuff. I don't like being in the building much either.
__________________