The only time I have ever lost a moly element was due to my own stupidity, of which I have an ample amount. I load cullet as well as batch . It you want to see something really blast around, try throwing in an entire color rod you don't like. My best understanding was that in an SiC, if a piece of cullet sticks to the element, It's toast and that it's not the cullet popping that does it damage at all. It's the chemical reaction.