I will gt the elements shipped by the end of the week Lawrence. Steve says you should have more spare straps than I was going to send. I suggest 20 in that case. The schematic you are looking for is in the Ark of the Covenant. ( there really really really isn't one).

I also did have yet another bussblock issue with my furnace two days back , coming in to a bank of elements being down and had to replace one on a Sunday. Spares are good. It's the second time in two years doing the same one in the transformer. I had to cut the cables back about eight inches. Steve said I'm the only one to ever have transformer issues. My straps after two years look like they are brand new on the other hand.

You are doing a great job on that furnace.