The differences are hard to see in the ads. Diamond concentration per sq inch is really important and how the diamond is bonded to the metal- either resin or sinter metal bond. I don't actually know if Jersey makes a band saw blade but if they do you have to check out process either way. Either way it's a very useful thread and I'm going to move it to "classics" since it's such a persisting search.