Dave Bross is on a distinguished road
Many thanks Pete! It never would have been possible to get something so incredibly nice on the first try without a whole lot of help.

More questions of course....

On the batch I just melted...

If I wanted to take the COE down to the 92-3 range to fit Fenton stuff, up to 96 to fit Spectrum, or even go completely nuts, kiss durability goodbye, and try taking it up around 102-4 to match Moretti, how would I go about it?

Would adding certain amounts of silica or soda be enough, or do the other things need to change on a percentage basis along with that?

What is the Corning Protocol?

I did melt it at 2200 after I got all the batch loaded and I'm pretty sure I would have screwed it up if I had tried at 2000.