Franklin: everything lowers the melt point of silica. Everything that does it extracts a price. At a certain point it won't turn back to a recognizable solid. There are defining limits. It is what the entire science of glass chemistry is about.
When do materials with no defined softening point get pissed off?

That's the short version.