Did a melt today.
224g yellow iron oxide and 114g red copper oxide mixed in 50# SP87.
This recipe was courtesy of Ed Branson in western Massachusetts, although his had red iron and black copper.
Seems to be a nice turquoise-green.
The one at the top was my previous melt with a tiny bit of cobalt for the light blue.
******************
The top one actually looks like an intense copper glass to me Josh and the bottom certainly looks like iron and copper. Good Job!