Micheal-

Thank you for your response.
the mold we are having particular issues with has been re-corked three times now, and the majority of the scratches are in the center of the piece.

They are faint, but noticable, and fairly consistant. We blow into it about 1 every 10 minutes. some scratches are deeper than others.

How many layers of this very fine cork do you use? it's less abrasive than a 40/80? What effect do you think begining with 40/80 and then finishing with a layer of 80/200 would be?