That's about my take on it too. Judging only by the off gassing alone the new Oceanside is either just their sheet formula or the original Studio, and I'd prefer not to cook any of it.

I didn't really run into issues with either Premium nor the New Formula Studio, but judging by how long it took to get the Flake, I'm not planning on waiting it out for something better.

D&L is the only US distributor for the flake right now. While I've had great experiences with them, they're primarily a wholesaler with steep demands. That will be problematic for any small scale buyers.