I am using a product called Resilience that is a dental compound. I once got a 5kg box as a "sample". I still like using it between 20 micron alumina and cerium but don't do near as much polishing as I once did.

Since I have finally decided to keep going until at least when I run out of glass or the crucible signs off, I am cleaning up my cold work area for whatever comes, so there will certainly be a need for touch ups if nothing else.