You can bet yo' ass I'm using the gloves and respirator. I'll be keeping my silica snots in the pots, not my lungs, thank you.

Even if my no antimony version is OK I'll keep using the gloves to develop the habit for when it gets to be color play time.

I'm still only doing 15 pounds at a time so I can keep the dusting down to very minimal levels. If I was doing hundred pound lots I would go for the tyvek suit and ventilation.

I just did surgery on my digital camera, and the patient actually survived, so I'll get some pics.