Brick for holding elements

I have used soft brick and made groves in them to hold my heating coil. Each time my elements fail I have to clean out the groves and rip out the elements etc before reinstalling new ones. My soft brick can’t take much more abuse. Jordan used kastolite 30 to make holders for the coils. Is there a more robust brick you can cut groves in to hold the elements.?
Franklin
Reply With Quote
  #2  
Old 05-16-2019, 07:59 PM
Shawn Everette Shawn Everette is online now
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 195
Shawn Everette is on a distinguished road
More robust brick? Yes. Readily cut grooves? No.

If you have the resources encasing the coils in quartz tube can do wonders. Otherwise Dudley sells a goop that's pretty good at keeping elements in place.
Reply With Quote
  #3  
Old 05-17-2019, 10:06 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,862
Franklin Sankar is on a distinguished road
Thanks.
Franklin
Reply With Quote
  #4  
Old 05-17-2019, 12:34 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,028
Pete VanderLaan is on a distinguished road
I suspect you have a commercial kiln Franklin. The brick for the bulk of those are under engineered for the job in my opinion. Often, it's a converted ceramic kiln for as little as bisque fire but even at cone 10 the kiln is usually shut down ( by the cones themselves) so the high temp soaks that you need, never happen at all. I don't think the materials were ever envisioned to be in service 24/7.
The one time I tried building something like what Jordan proposed, I used a 2600 brick and cut shim bricks on the saw so that each layer of brick had this smaller shim leaving a gap enough for an element. It was larger, about 48x 28 inch and had seven elements. It did work well but I eventually dismantled it when we moved. Using the shim approach did take a mess of mortar but was easier in my mind to build.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 05-17-2019, 04:09 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,862
Franklin Sankar is on a distinguished road
Thanks Pete. It is as you describe but using what material I could get. I like your design but I can get 2200 soft brick or hard brick. No 2600. Have to keep rebuilding every so often. Because I can only use soft brick and 6” fiber top bottom and sides.
The cavity is 10” deep and 11” diameter.
I hope Jordan did some more work on his design and can share the test results.
My fear for his design is that it may want to crack in the high furnace heat. But since it is ramping up down slowly it may be ok. Don’t know.
Franklin
Attached Images
File Type: jpg image.jpg (19.8 KB, 22 views)
Reply With Quote
  #6  
Old 05-17-2019, 08:06 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,028
Pete VanderLaan is on a distinguished road
you can't make it last with substandard materials. Simple as that.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 05-18-2019, 10:58 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 3,862
Franklin Sankar is on a distinguished road
Very true
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 09:20 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.