Before, way before. The final nail in the coffin came when a renter decided to do a plaster cast in it ... and forgot to put the thermocouple back in.
Reply With Quote
  #52  
Old 04-18-2019, 01:20 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,066
Pete VanderLaan is on a distinguished road
well, given the construction, eventually the room would come up to temperature if you know what I mean.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #53  
Old 04-18-2019, 01:47 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 175
Shawn Everette is on a distinguished road
I did a complete overhaul, 20 gauge sheet metal seems like a poor choice for framing material. That one was ancient, still had the old rheostat controls.
Reply With Quote
  #54  
Old 04-18-2019, 01:57 PM
Richard Huntrods's Avatar
Richard Huntrods Richard Huntrods is offline
Registered User
 
Join Date: Aug 2003
Location: Vancouver Island
Posts: 1,155
Richard Huntrods is on a distinguished road
Quote:
Originally Posted by Randy Kaltenbach View Post
I've been thinking about this. How hot would the exterior likely reach? I don't want to skin it with galvanized metal if it's too hot.
Randy, sheet metal is a terrible skin. The expanded steel mesh is much better as it doesn't become a radiating surface like the sheet.

My annealer is a 17" kiln, brick with 1/4" frax and then sheet metal. At 920 you can get an instant 2nd degree burn if you touch it with your knee. (ask me how i know!).

My furnace has more insulation (1" rigid board, 2" roxul) and expanded mesh. At 2100F the exterior is 150F (measured). Hot, but you can touch it and not get burned. I've put my hand on it for 20-30sec without ill effect.

Part of that is the much greater insulation around the brick 'hot zone', but the expanded mesh is just a much superior "skin". If you worry about fiber 'bits' in the air, just spray paint the thing with black hi-temp engine paint. Works wonderfully.
Reply With Quote
  #55  
Old 05-27-2019, 01:41 PM
Randy Kaltenbach's Avatar
Randy Kaltenbach Randy Kaltenbach is offline
Registered DancingChicken
 
Join Date: Aug 2003
Location: Calgary, Canada
Posts: 973
Randy Kaltenbach is on a distinguished road
So ...

I read Dudley's GREAT material, picked up a drafting software package and was well on the way to figuring out optimum soft brick layout etc. When doing a quick supplier check on some materials, I stumbled across an old Skutt model K top load ceramics kiln for $300, called the guy and talked him down to $220 CDN, moved it into my garage, and now I'll simply fix it up (needs some TLC) and add a controller.

I may modify it to add a bead/parts door.

Not optimal but WAY cheaper! At least it's a start.

Thanks for all the suggestions and advice.
Reply With Quote
  #56  
Old 05-27-2019, 03:12 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,066
Pete VanderLaan is on a distinguished road
It's much better than starting with a large mailbox.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #57  
Old 05-27-2019, 07:24 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 916
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Randy Kaltenbach View Post
So ...

I read Dudley's GREAT material, picked up a drafting software package and was well on the way to figuring out optimum soft brick layout etc. When doing a quick supplier check on some materials, I stumbled across an old Skutt model K top load ceramics kiln for $300, called the guy and talked him down to $220 CDN, moved it into my garage, and now I'll simply fix it up (needs some TLC) and add a controller.

I may modify it to add a bead/parts door.

Not optimal but WAY cheaper! At least it's a start.

Thanks for all the suggestions and advice.
Great starter kiln for sure. Parts door is definitely a valuable addition.
Reply With Quote
  #58  
Old 05-28-2019, 05:57 PM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is online now
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 935
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
It's much better than starting with a large mailbox.
I know you can build this with a manual controller for less then a hundred dollars. Honestly I built this kiln about 20 years ago and it still gets used regularly. Some fiber insulation, a 15 amp element and oven switch. It’s hard to beat simplicity.
Attached Images
File Type: jpeg 1D43242F-19C2-4F5D-8902-C35D76F4288C.jpeg (40.8 KB, 34 views)
Reply With Quote
  #59  
Old 05-29-2019, 09:17 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,066
Pete VanderLaan is on a distinguished road
I had one here for years built out of a stainless dishwasher. When replaced, it was put in storage, not chucked.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #60  
Old 05-29-2019, 10:21 AM
Sky Campbell's Avatar
Sky Campbell Sky Campbell is online now
Registered User
 
Join Date: May 2002
Location: Gainesville FL
Posts: 935
Sky Campbell is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
I had one here for years built out of a stainless dishwasher. When replaced, it was put in storage, not chucked.
That’s brilliant. The restaurant dishwashers have a guillotine style door. Save one of those from the scrapyard and make a nice kiln out of it. I’m going by my favorite picking place today I might just have to see if there’s one laying around. I was once told “you must have a 100 kilns” I figure one more won’t hurt anything.
Reply With Quote
  #61  
Old 05-29-2019, 10:52 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,066
Pete VanderLaan is on a distinguished road
we regularly took that lab unit up to 1500F which was hard on the hinges but that was the only issue. I used it primarily for fusing Mary Beth's stuff and for heating up color rods. It was still working just fine when I took it out of service after around 20 years. I've seen larger ones made out of restaurant refrigerators. I like that sort of stuff.

John Nickerson built one at one point with Eisenglass or pyrex ( I forget) in the front and he would take stuff up to slumping temps and then manipulate the piece with two rods he had stuffed in the openings like on a sandblaster.

The good old days when you couldn't buy tools. John Bingham and I built virtually all of the big roughers we used. It would take an old Lang base and rework it. Nick did some fabulous drawings of how to do that for the Hot Glass Information Exchange that we published back in 1979. Those drawings are clear as a bell. We made the wheels from drops in bridge abutment steel and those beasts were up to 2 inches thick by a minimum of 30 inch diameter. They weighed up to five hundred pounds and I think cost about 100 dollars each after being clear faced on both sides with a center punch of 1.29. You needed about five friends to change a wheelhead.

"You must have 100 kilns" Amen to that.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:39 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.