Fin molds

Does anyone have any experience with the Jim Moore fin molds with the interchangeable fins? I'm considering buying one and would like to know if anyone has used them and an opinion of how they work and hold up, i.e. do the fins warp over time, how difficult is it to change over etc. I've worked with one or seen one up close at another studio or in his booth at GAS so I never got a chance to actually kick the tires on one.
Reply With Quote
  #2  
Old 08-17-2018, 04:02 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 20,748
Pete VanderLaan is on a distinguished road
Your gather needs to be perfect , upright and centered when you use it. So, operator experience required. I use Steinerts these days when ever I do this sort of stuff, which is really rare. Michael Christman had some of these things for sale in Arkansas a few years back. They looked pretty rusty.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 08-17-2018, 04:26 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,655
Jordan Kube is on a distinguished road
Jerry Kung makes some really excellent inside and outside fin molds in several sizes. You can probably get a hold of him via instagram @jlinhsienkung or facebook. You can scroll down his instagram profile to see some of them.
__________________
WWUD? Think for yourself.
Reply With Quote
  #4  
Old 08-17-2018, 04:33 PM
David Russell David Russell is offline
Registered User
 
Join Date: Jul 2008
Location: South Carolina
Posts: 198
David Russell is on a distinguished road
The jim moore fins hold up well and are sturdy. Easy and relatively quick swap out. Lift off the retaining ring and the ribs slide out easily.
Reply With Quote
  #5  
Old 08-17-2018, 04:35 PM
Rich Simmons's Avatar
Rich Simmons Rich Simmons is offline
Registered User
 
Join Date: Aug 2018
Location: California
Posts: 30
Rich Simmons is on a distinguished road
I've never liked them.
What are you going for? - Pumpkin's, there's better options out there. The normal fin molds, I use for Venetian and are just fine I have Jim's "8 Facet
3-7/8" tall x 3-1/2" wide at top and 5-1/2" wide at base"

I don't think the detachables are worth the $$. My 2 cents...
Reply With Quote
  #6  
Old 08-19-2018, 09:51 AM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 523
Art Freas is on a distinguished road
I got them with the shop when we bought the shop. The are nice if you are a glassblower, not for make your own pumpkin events. The comments about being centered and having the correct gather are right on, those things matter with this mold since there is nothing to stop uneven blowing between the fins. The flexibility to change the number of fins and the shape of the fins is really nice. The fins are holding up fine. The are easy to change over so no drama there.
Reply With Quote
  #7  
Old 08-22-2018, 10:50 PM
Paul Thompson Paul Thompson is offline
Registered User
 
Join Date: Apr 2007
Location: Hygiene CO
Posts: 189
Paul Thompson is on a distinguished road
Quote:
Originally Posted by John Riepma View Post
Does anyone have any experience with the Jim Moore fin molds with the interchangeable fins... .
They work fine. It's possible to blow too much and get wrinkles on the inside. I use them for merletto (sp?). The fact that it doesn't always turn out is more a reflection on my meager skills.
__________________
"You don't have to be a very good glassblower when you can fix stuff" -- Richard Royal
Reply With Quote
  #8  
Old 08-23-2018, 02:15 AM
Rich Simmons's Avatar
Rich Simmons Rich Simmons is offline
Registered User
 
Join Date: Aug 2018
Location: California
Posts: 30
Rich Simmons is on a distinguished road
Quote:
Originally Posted by Paul Thompson View Post
They work fine. It's possible to blow too much and get wrinkles on the inside. I use them for merletto (sp?). The fact that it doesn't always turn out is more a reflection on my meager skills.
I find the price too high. If you have even meager skills at welding you can save a lot of money. Meager skill can also be attributed to a host of glass blowing failures, we all start out meager - practice then crash, practice then wonky, character building.. .

I made something like this for under $50 What bugs me about about Jim's molds is that they come with one set (Straight, etc) if you want different shapes it's another $200 for each set.
I don't know about you, but what Pete spoke about setup is everything, and he said is spot on, only thing he didn't mention is (and I don't know if this is right or wrong) technique is you gotta push the bubble waay down the piece and keep those sides overly thick.
Attached Images
File Type: jpg Optic_Molds_Spider.jpg (21.4 KB, 21 views)

Last edited by Rich Simmons; 08-23-2018 at 09:46 AM.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:58 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.