Powder booth fan

Building a powder booth. Have it all figured and built except I need a better fan. Looking to use a 12V DC radiator fan. I would like to be able to adjust the fan speed. Do I need a PWM with it or with a DC motor can I just use a potentiometer?
Reply With Quote
  #2  
Old 07-04-2020, 05:50 PM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Stanwood, WA
Posts: 137
Eric Trulson is on a distinguished road
Yeah, you can control a DC motor's speed with a potentiometer directly, no need for PWM.

That potentiometer is going to have to dissipate whatever power is being drawn away from the fan, so the pot and surrounding wiring may heat up if the booth uses a larger fan and it's left running on a low setting for a while. I doubt it will actually be an issue, just something to be aware of.
Reply With Quote
  #3  
Old 07-05-2020, 10:10 AM
Brian Graham's Avatar
Brian Graham Brian Graham is offline
Registered Abuser
 
Join Date: Mar 2004
Location: Akron - Ohio
Posts: 546
Brian Graham is on a distinguished road
This is the Dayton blower I use for powder and fuming. I have it connected to a plastic chamber - foot pedal operated. It moves a lot of air fast! Expensive unit - I found mine used for the price of good beer!
Attached Images
File Type: jpg blower 1.jpg (44.5 KB, 31 views)
File Type: jpg blower 2.jpg (32.4 KB, 19 views)
__________________
The revolution will not be televised.
Reply With Quote
  #4  
Old 07-06-2020, 12:52 AM
Art Freas Art Freas is online now
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 670
Art Freas is on a distinguished road
Built one that collapses and lays flat. Uses a HEPA filter that removes and then a dust collector hose that directs the filtered air up the hood. Used hinge pins to take hold the panels together.
Reply With Quote
  #5  
Old 07-06-2020, 07:11 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,034
Pete VanderLaan is on a distinguished road
Powder booths aren't really the same as fuming chambers. The powder only gasses when in direct contact with the glass piece. I doubt it needs the same high velocity.
The other thing about such chambers is that it needs to startup about three seconds before you actually make contact in either environment. Otherwise, it will go where it goes. The only powders that I think cause any real problem are the lead arsenates. I suspect that the basic air you breathe in your studios is equally as great an issue as booths. I see very few well vented studios.

Keep in mind glass workers are dying of Alcohol and tobacco and soon... covid 19 but not so much from this sort of stuff.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:05 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.