Casting a new crown.

I'm looking for some advice. I am building a new furnace and looking at my old crown I see that the skin it is peeling in layers.
Are used to cast a light 30. Are there any recommendations for a crown that would last longer without peeling?
Reply With Quote
  #2  
Old 07-12-2017, 02:18 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,212
Eben Horton is on a distinguished road
Can't beat castolite 30 imho..... crowns are meant to be replaced every 10-15 years I think.

That said, a friend used huge silicon carbide kiln shelves as a crown and swears by them.
Reply With Quote
  #3  
Old 07-12-2017, 04:15 PM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 805
Kenny Pieper is on a distinguished road
Quote:
Originally Posted by Mike Kaplan View Post
I'm looking for some advice. I am building a new furnace and looking at my old crown I see that the skin it is peeling in layers.
Are used to cast a light 30. Are there any recommendations for a crown that would last longer without peeling?
If you are melting batch I would recommend that you use something harder and more durable than cast a lite 30. Ask your refractory source. There are so many options now days.
Reply With Quote
  #4  
Old 07-12-2017, 10:42 PM
Mike Kaplan Mike Kaplan is offline
Registered User
 
Join Date: Apr 2002
Location: cleveland ohio
Posts: 208
Mike Kaplan is on a distinguished road
Thx for the advice. I always seem to forget to ask the experts first.
Reply With Quote
  #5  
Old 07-13-2017, 08:57 AM
Mike Kaplan Mike Kaplan is offline
Registered User
 
Join Date: Apr 2002
Location: cleveland ohio
Posts: 208
Mike Kaplan is on a distinguished road
I would say this crown lasted 3 yrs and i use cullet. It didnt crack but it is pealing
Reply With Quote
  #6  
Old 07-13-2017, 10:35 AM
Justin Zotynia Justin Zotynia is offline
Registered User
 
Join Date: Aug 2009
Location: Bushkill, PA
Posts: 56
Justin Zotynia is on a distinguished road
I used kastolite 30 for my crown and used cullet worked well no peeling. maybe every furnace environment is different due to design. don't know just that it worked for me.
Reply With Quote
  #7  
Old 07-13-2017, 10:40 AM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,590
Jordan Kube is on a distinguished road
I would use something a little heavier duty than Kast-o-lite. Some people have good success with it. It doesn't seem to be the case in your furnace. Make sure you mix thoroughly and to manufacturer's instructions as well.
__________________
WWUD? Think for yourself.
Reply With Quote
  #8  
Old 07-13-2017, 11:44 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,212
Eben Horton is on a distinguished road
I'd bet you a case of beer that when you made your crown 3 or 4 years ago, you made th mix too wet. If you mix it right, it will last a long long time. Mix it wet and the casting will be brittle and won't last. I learned this with glory hole and furnace doors. Also, make it thick. At least 4 inches and give it a nice arch to give it strength
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 03:43 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.