caged Pieces

I wish to do some caged pieces. Other than copper what other metals do you have success with blowing into. My goal is to include the metal into the piece. as in a lamp shade. I use spruce pine Thank you.
Reply With Quote
  #2  
Old 07-03-2017, 01:30 PM
Mike McCain's Avatar
Mike McCain Mike McCain is online now
I am a cog
 
Join Date: Jan 2013
Location: Maui
Posts: 369
Mike McCain is on a distinguished road
I've worked in shops that used steel cage frames that were sprayed with black grill paint. Thin enough gauge that the steel had some bend when you squoze it. The frames were at room temperature, and we didn't blow too far past the cage. If the bubble blew out too far, and started to wrap around the steel, it would break on annealing. If the glass bulged out a bit, which is the whole point, seemed fine.
Copper is the only metal I know of that can be cased in glass without much stress on annealing, but you gotta be quick to cover the copper if you want that sweet pink hue and not a charred mess.
What I like, is to drop a cookie on to some copper sheet (forget foil, go thick. Carbondale copper has many thicker gauges for your shopping pleasure.). Drop the cookie on the copper sheet. Go get another gather an make a post. Use your Dave Patchen patented tagliols and flip the cookie. Sandwich the copper and your on your way to making some attractive baubles.
__________________
This is your burning hand; it's right here.

Last edited by Mike McCain; 07-03-2017 at 01:38 PM.
Reply With Quote
  #3  
Old 07-03-2017, 01:44 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 19,564
Pete VanderLaan is on a distinguished road
In Mexico they used tin cans that were first cut with a torch. THey were really pretty good at making different shapes with the bigger cans. I have no idea if they are still around. I would imagine they would be, You had only one chance to blow the mold and get rid of the thing.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 07-04-2017, 09:49 AM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Please Disperse
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 1,878
Greg Vriethoff is on a distinguished road
I've experimented with sterling silver in the past. Thick castings, not blown. Silver doesn't hold-up structurally as well as copper. If I were going to explore this again I would try and use fine silver. Higher melting point. Probably wouldn't make that much of a difference, but who knows what'll happen. Gold can be used as well, but same issues as silver in addition to $$$.

Copper's pretty much the go to for cost, durability, and "compatibility." Steel is more a matter of technique. I've worked with some people that do some reckless stuff with steel and glass. It's a lot of "getting away with it" and I seriously doubt pieces with steel inclusions will stand the test of time.
__________________
"It's such a fine line between stupid and clever." - David St. Hubbins
Reply With Quote
  #5  
Old 07-04-2017, 10:41 AM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: hills of Tennessee
Posts: 1,286
Tom Fuhrman is on a distinguished road
In the 60's and 70's we used steel frames for making thousands of caged light fixtures. Sinclair Glass in Indiana, Super Glass in Brooklyn and many others. As Pete stated , many of the Mexican factories did the same. Frames were strip steel and spot welded in mass production situations.
During that era, "Mediterranean" theme/Spanish, etc. and Mexican decors were very popular so that was what was selling. I even used to have some large planters that were produced this way. About 12" tall X 14" diameter and totally open on the one end where they were cut off and ground. About 30 years ago I had hundreds of these fixtures I bought as an entire warehouse closeout and ended up selling them to a chain of Mexican restaurants.
Reply With Quote
  #6  
Old 07-04-2017, 11:35 AM
Dan Vanantwerp Dan Vanantwerp is online now
Registered User
 
Join Date: Apr 2017
Location: Bozeman, MT
Posts: 118
Dan Vanantwerp is on a distinguished road
I'm still kind of fascinated by the blown boro post and wonder what that glass can withstand...besides METEORITE incusions!
Reply With Quote
  #7  
Old 07-05-2017, 03:25 PM
Pamela Sherwood Pamela Sherwood is offline
Registered User
 
Join Date: Aug 2015
Location: Palo Alto
Posts: 14
Pamela Sherwood is on a distinguished road
I have made fine silver cages. It's best not to work in the glory hole for a long time afterwards, but it can be done. And fine silver is much, much better than sterling.

For copper - you can use wire or mesh. Fine silver mesh too, but it's expensive.
Reply With Quote
  #8  
Old 07-05-2017, 04:39 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,544
Jordan Kube is on a distinguished road
KT Hancock of Spiral Arts fame has been doing a bunch of really neat blown steel cage work pieces. Her most recent work can probably be found on Instagram.
__________________
WWUD? Think for yourself.
Reply With Quote
  #9  
Old 07-13-2017, 11:23 PM
Mike McCain's Avatar
Mike McCain Mike McCain is online now
I am a cog
 
Join Date: Jan 2013
Location: Maui
Posts: 369
Mike McCain is on a distinguished road
Spraying Stannous Chloride on Gold and Silver foil help those precious metals 'pop' and can help justify the price tag.
__________________
This is your burning hand; it's right here.
Reply With Quote
  #10  
Old 07-14-2017, 02:22 AM
Eric Trulson Eric Trulson is offline
Young Turk
 
Join Date: Sep 2014
Location: Lowell, MA
Posts: 69
Eric Trulson is on a distinguished road
Quote:
Originally Posted by Mike McCain View Post
Spraying Stannous Chloride on Gold and Silver foil help those precious metals 'pop' and can help justify the price tag.
That is super fascinating. Do you usually dip/spray the stannous chloride on the foil beforehand, or do you apply it to the surface after it's been rolled up?

I'm assuming the extra shine comes about because the stannous chloride acts as a reducing agent and prevents the metal surface from oxidizing as much as it would otherwise. Not sure though.
Reply With Quote
  #11  
Old 07-14-2017, 02:30 AM
Mike McCain's Avatar
Mike McCain Mike McCain is online now
I am a cog
 
Join Date: Jan 2013
Location: Maui
Posts: 369
Mike McCain is on a distinguished road
I never thought of dipping the foil in a stannous bath. Could be cool. I just sprayed it, and the gold seemed to remain more than when on its own. Possibly the stannous 'filled the gaps' that come about. Interesting thought about the chemistry behind why it works. I don't know. All I can say is it makes it 'pop.'
__________________
This is your burning hand; it's right here.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 08:13 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2018, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.