Sluggish Electric Furnace--Possible Fix

If your electric furnace is more than eight years old, uses a Watlow Power Series SCR, and is excruciatingly sluggish, there's a function that can be disabled in the SCR which is likely the cause. The function is displayed as HCYC, and it was set up to solve a theoretical problem that never materialized. Instead, this function causes near-debilitating sluggishness.

A little backstory--Wet Dog Glass stopped using these SCRs after only using four of them 10 years ago when Watlow admitted that they use cheap current transformers because the vast majority of customers for this product use it for burst firing--not phase angle, and that the cheap current transformers were indeed the cause of the problem I was having. After having another brand new furnace fail to function properly, Watlow had me disable the HCYC function. That adjustment worked immediately. A few months ago, I remembered this fix when a furnace that previously functioned well began to drag on its way to melt temp after ten years of service. Since then I've helped a number of non-Wet Dog Glass furnace owners who were at wit's end over how slow the furnaces were, and those who found the HCYC function enabled and then disabled it reported that their furnace was like "a whole new animal!"

Attached is a .pdf file with instructions on disabling this feature.
Watlow Power Series_HCYC disable.pdf

Last edited by Eddie Bernard; 05-30-2019 at 05:23 PM.
Reply With Quote
  #2  
Old 05-30-2019, 06:31 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 920
Larry Cazes is on a distinguished road
Probably a hysteresis function
Reply With Quote
  #3  
Old 05-30-2019, 06:33 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,077
Pete VanderLaan is on a distinguished road
This goes straight to "Antiques and Classics". Thanks Eddie.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 05-30-2019, 08:52 PM
Rick Kellner Rick Kellner is online now
Registered User
 
Join Date: Jan 2004
Location: Hillsboro, OR
Posts: 160
Rick Kellner is on a distinguished road
Quote:
Originally Posted by Larry Cazes View Post
Probably a hysteresis function
I concur. That's exactly what came to mind when I saw the acronym.
Reply With Quote
  #5  
Old 05-30-2019, 09:55 PM
Lynn Read Lynn Read is offline
Registered User
 
Join Date: Aug 2008
Location: Portland, OR
Posts: 17
Lynn Read is on a distinguished road
Hi Eddie

Thanks for making this suggestion at the GAS conference. After tuning off this alarm it seems my furnace is running about 10 % lower on output. I was able to reach higher melt temps with the same output.
Reply With Quote
  #6  
Old 05-31-2019, 01:35 PM
Richard Huntrods's Avatar
Richard Huntrods Richard Huntrods is offline
Registered User
 
Join Date: Aug 2003
Location: Vancouver Island
Posts: 1,156
Richard Huntrods is on a distinguished road
Some modern controllers have an 'auto tune' function that saves data on the performance of the controller over time, and can adjust the response of the controller over time if it sees a change. (i.e. elements getting old and response to X power slowing down).

It works pretty well until you do something stupid, like maintenance with the shutoff switch blocked (i.e. in the off position) while the system is running. In my case it kept trying to hold the temp setting (1900F) while the door was open and temp was falling. After I was done and returned things to normal, I had a severe case of "temperature overshoot" for many days until the system auto-tuned itself back into normal behavior.

But the tuning curve can get in the way and it sounds like this is a quick way to reset the data and restore factory response times.
Reply With Quote
  #7  
Old 06-01-2019, 06:24 AM
Eddie Bernard Eddie Bernard is offline
Registered User
 
Join Date: Jan 2015
Location: NC,
Posts: 5
Eddie Bernard is on a distinguished road
The HCYC prompt stands for “Half Cycle Line Loss.”. The theory as explained to me by Watlow was that if supply voltage on any phase was disrupted to the degree that it lost half the cycle, meaning the positive or negative half of the sine wave, the resulting DC component could have caused damage to the transformer. As a matter of fact, these very instructions originally stated that the user should not disable the HCYC function when the SCR was firing into a transformer. I retyped it and added a few notes to clarify the steps to get to the setup and factory pages based on feedback from some users who went through the process. I did speak with Watlow in March and asked them again to confirm that we should ignore the note about not disabling HCYC when using a transformer, and they did confirm without hesitation.
Reply With Quote
  #8  
Old 06-01-2019, 07:25 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,077
Pete VanderLaan is on a distinguished road
Is it not the case that all Moly SCR relationships fire into the transformer?
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 06-01-2019, 12:31 PM
Eddie Bernard Eddie Bernard is offline
Registered User
 
Join Date: Jan 2015
Location: NC,
Posts: 5
Eddie Bernard is on a distinguished road
As far as I know, the vast majority of furnaces using Moly-D’s in our art glass community also use transformers. I know some of you who have been on CraftWeb for years will recognize some of the conversation Steve Stadelman used to have with others here—It’s not exactly necessary to use transformers, but it’s the responsible thing to do in terms of power factor (for the sake of the power grid) when the resistance of the elements added up in series won’t be enough to resist full line voltage without self-destructing. Some people use 120V single phase and put the elements all in series and let the phase angle SCR take care of the discrepancy in voltage needed, and there are also interesting arrangements that can be done with contactors to change the element arrangement from Series Wye to parallel Wye to Series Delta to Parallel Delta as they heat up. That’s a lot to go through to avoid using a transformer.

Another key advantage we have with transformers is the safety it can provide the user when it is an isolation type with the X0 tap not grounded and secondary voltage lower than 48V. For production shops where the door is opened more frequently than the furnace can recover the heat lost while open, the user can safely bypass the door safety limit switch without risk of electrocution. This is known as SELV, or “Safety Extra Low Voltage.”. The elements remain energized while the user is gathering glass from the furnace.
Reply With Quote
  #10  
Old 06-01-2019, 02:15 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 21,077
Pete VanderLaan is on a distinguished road
I don't know of any that use line voltage. I always viewed that as the downside of SiC. When Steve was building the very early ones, it was all salvage transformers which were virtually all 440V. One could trick the transformer and run 240V into it and it created two 120V taps and one 60V tap which worked great with the 6/12 type elements drawing 20 Volts. The downside was serious fragility.

My furnace, which we put together back around 2001 did not have a kill switch. I tend to think any commercial unit would be nuts to not have one just for the liability. It did not take long for commercial transformers from Marcus to become mainstream. Then the beefier 9/18 elements could be used easily and secondary voltage could collapse to 36V.

While they are still built a fair amount, it never bcame the hot tool I thought it would. The initial belief was that it would be so low maintenance and it was far from that as it turned out. Then. Electric rates where I live made it impossible to justify not using Propane or natural gas. I prefer the gas actually although it's not as safe. I just can't get the colors I want with moly. If I ran electric now, a 28 inch pot would cost close to 3K per month to run. Propane is about $600 and I think that's a lot.
__________________
Where are we going and why am I in this basket?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 05:05 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.