High precision glass polishing w ketchup - really!

Ketchup containing micro-sized cerium oxide

Quote:
Abstract

Due to the advantages over conventional polishing strategies, polishing with non-Newtonian fluids are state of the art in precision shape correction of precision optical glass surfaces. The viscosity of such fluids is not constant since it changes as a function of shear rate and time. An example is during the shape correction by polishing with pitch or ice, where pitch flows slowly under its own weight and acts like a solid body during short periods of stress as its viscosity increases. One approach is to use thixotropic fluids like ketchup to reduce the roughness by polishing, without changing the shape of the sample. Tomato ketchup shows a time-dependent change in viscosity: the longer the ketchup undergoes shear stress, the lower is its viscosity. Therefore, in this article, a new processing is put forward to polishing glass surfaces with ketchup containing micro-sized Ce2O. Besides conventional ketchup, curry ketchup and an organic product were tested as well. An industrial robot onto the work piece surface guides the polishing head. The different types of ketchup are compared by means of roughness and shape accuracy and the potential regarding to manufacture high-precise optical glass surfaces.
(2020) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
https://www.spiedigitallibrary.org/c...67.short?SSO=1
Reply With Quote
  #2  
Old 07-25-2020, 05:45 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,199
Pete VanderLaan is on a distinguished road
I'll bet it stains my shirt as well as Panda Cerium.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 07-26-2020, 04:02 AM
Hugh Jenkins Hugh Jenkins is offline
Registered User
 
Join Date: Sep 2006
Location: Honoka'a, HI
Posts: 1,007
Hugh Jenkins is on a distinguished road
I like the addition of baby shampoo better. Really.
__________________
Aloha, Hugh
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:29 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.