Scale in cullet

If you have bits of scale in the cullet for remelting. Does it drill holes in the pot, or affect the small pot.
Franklin
Reply With Quote
  #2  
Old 07-18-2020, 07:05 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,050
Franklin Sankar is on a distinguished road
Ok I do it to practice sometimes.
Franklin
Reply With Quote
  #3  
Old 07-18-2020, 09:49 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,291
Pete VanderLaan is on a distinguished road
If your work is entirely clear, yes the iron tone will show. If you are adding color, you'll likely never see it at all.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 07-18-2020, 10:54 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,050
Franklin Sankar is on a distinguished road
So it does not harm the pot. Donít care about coloring .
Franklin
Reply With Quote
  #5  
Old 07-18-2020, 12:50 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,291
Pete VanderLaan is on a distinguished road
It does not harm the pot.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #6  
Old 07-18-2020, 01:03 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,050
Franklin Sankar is on a distinguished road
Great. Thanks
Franklin
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 04:12 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.