New 50lb furnace for color, best advice to start

Just ordered a Vulcan II crucible kiln, for my studio. I would really like to get advice on pretty much anything and everything that any one has to offer as far as maintenance, trouble shooting, and best ways to START batching some color. I currently batch spruce pine in my main furnace. Thank you everyone in advance.
Reply With Quote
  #2  
Old 07-09-2019, 11:26 AM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 696
Shawn Everette is on a distinguished road
Ditch the electric and get a gas furnace?
Reply With Quote
  #3  
Old 07-09-2019, 02:11 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,285
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Shawn Everette View Post
Ditch the electric and get a gas furnace?
****
And aren't we such a big help....

Get a copy of Glassnotes IV and read the section I wrote on batch. Then read the Section Frank Wooley wrote on annealing. Get a copy of Volf "Chemical approach to Glass" and a copy of Weyl "Colored Glasses". Then try to buy a copy of the Willhelm Schmidt formulas from the Thuringen Factory 1925 translated by Finn Lyngaard. Then get Henry Helmer's "Secret book of batch formulas".

Then get rid of the electric furnace and go to gas... There's a lot you can't do in electric.

I'm actually considering rewriting the Schmidt book and converting every formula to being a 96. L.E.C. I am wondering if that's copyright violation.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 07-10-2019, 08:46 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,717
Jordan Kube is on a distinguished road
I like to use an 8' x 8' grow tent as a batch room. *Just* fits everything you need and you can roll it up and throw it away when you're done with it. Always seemed like a better idea than having to deep clean some space after you were done.

Details in this thread: http://talk.craftweb.com/showthread.php?t=11837
__________________
WWUD? Think for yourself.
Reply With Quote
  #5  
Old 07-15-2019, 12:04 PM
Paul Stout Paul Stout is offline
Registered User
 
Join Date: Aug 2015
Location: Tucson AZ
Posts: 18
Paul Stout is on a distinguished road
"Get a copy of Glassnotes IV and read the section I wrote on batch. Then read the Section Frank Wooley wrote on annealing. Get a copy of Volf "Chemical approach to Glass" and a copy of Weyl "Colored Glasses". Then try to buy a copy of the Willhelm Schmidt formulas from the Thuringen Factory 1925 translated by Finn Lyngaard. Then get Henry Helmer's "Secret book of batch formulas".

A mere $3k in books in today's money, lol. But probably worth it. Henry Halem gave me his copy of Weyl's book and Im forever grateful. Glass Notes is the best place to start but you will have many more questions. I can't really speak on electric, our color furnace is natural gas. I'm surprised there's not a "DIY Colored Glass" by Pete Vanderlaan, available. Seriously though i would be very interested in seeing a rewrite of Schmidt's formulas.
Reply With Quote
  #6  
Old 07-15-2019, 01:49 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,285
Pete VanderLaan is on a distinguished road
Indeed. Maybe you and at least eleven other people.

Igneous Glass reprinted Volf and I believe it was $200.00. Weyl is apparently currently out of print but can be found used as an ugly softback. Hardbacks are quite rare. I know of a copy of Schmidt being auctioned on Ebay right now for $100.00. Helmer is available through Igneous. $100.00 I think.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #7  
Old 07-15-2019, 02:06 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,285
Pete VanderLaan is on a distinguished road
Here apparently is a new printing of Weyl fairly cheap from ebay

https://www.ebay.com/sch/i.html?_fro...roach+to+glass

I don't know where the cover shot came from. There's not much info but one of them claims to be brand new and is the cheapest.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 08-14-2019, 09:00 AM
Rollin Karg Rollin Karg is offline
Registered User
 
Join Date: Apr 2002
Location: Kechi, KS
Posts: 924
Rollin Karg is on a distinguished road
Quote:
Originally Posted by Ken Miller View Post
Just ordered a Vulcan II crucible kiln, for my studio. I would really like to get advice on pretty much anything and everything that any one has to offer as far as maintenance, trouble shooting, and best ways to START batching some color. I currently batch spruce pine in my main furnace. Thank you everyone in advance.
Start small and simple(15pound pot), cobalt added to your batch is a good place to start. Ive been making color for a long time in both electric and gas furnaces. Started with a small 10 pound pot and used as big as 1000 daytank. Currently using both gas and electric to make colors. There is still a world of info here, just dig in.

Is Perrysburg in Ohio ?
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 11:34 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.