Working solo to Make a goblet

Bill G is my hero for working solo . Is there any one who works solo making a goblet but with a different method to Bill.
Franklin
Reply With Quote
  #2  
Old 10-15-2020, 03:04 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 723
Art Freas is on a distinguished road
Not goblet but we have a person that rents time at our shop that does incalmo and paperweight incalmo vases solo. Amazing to watch.
Reply With Quote
  #3  
Old 10-15-2020, 06:06 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,302
Pete VanderLaan is on a distinguished road
Working solo is all I've ever done, more out of necessity than anything else. That includes stemware.

With a garage, I know of very intricate work done solo. Otherwise , timing is really critical.

I just like it because I can always find my tools where I left them.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #4  
Old 10-15-2020, 07:51 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,050
Franklin Sankar is on a distinguished road
Thanks for the replies. So it seems that the difference is in the use of a garage.
The timing part is key for sure but recognizing the heat in the glass is not easy.
I need to keep it going and not shut down for such long periods.
Franklin
Reply With Quote
  #5  
Old 10-15-2020, 08:54 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 696
Shawn Everette is on a distinguished road
A garage is certainly helpful with multi piece work, but a will finds a way. Watching Toso with a killer gaffer and every assistant at the beckoning was a complete contrast to Bill alone with a hot box at his feet. Good glass helps too...
Reply With Quote
  #6  
Old 10-15-2020, 09:32 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,777
Eben Horton is on a distinguished road
A small color box that has a top loading door is far more useful than a garage if you are blowing solo.
__________________
<eben epoiese>
Reply With Quote
  #7  
Old 10-16-2020, 08:18 AM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,050
Franklin Sankar is on a distinguished road
Ok how about this. Can you share a link illustrate your technique?
Franklin
Reply With Quote
  #8  
Old 10-16-2020, 09:00 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,302
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
A small color box that has a top loading door is far more useful than a garage if you are blowing solo.
****
The other tool I've seen used was a wire hot box that had no top or bottom. You can hang up a piece and have the wire kiln surround the gathered glass at about 1150F and it keeps it ready while you work on some other part.

There must be Youtubes of these things. It's no state secret. We might be keeping it from Trinidad though.

Oh... and yes to that "good glass"
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #9  
Old 10-16-2020, 12:49 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 723
Art Freas is on a distinguished road
"A small color box that has a top loading door is far more useful than a garage if you are blowing solo."

Very true, thats what we have in our shop. Our solo blower puts the granny next to it. When he picks up for incalmo he puts the blow pipe in the granny, picks up the cup with a punty and then takes them both back to the hole.
Reply With Quote
  #10  
Old 10-16-2020, 01:37 PM
Tom Fuhrman Tom Fuhrman is offline
Registered User
 
Join Date: Apr 2002
Location: Lakeland, Florida
Posts: 1,480
Tom Fuhrman is on a distinguished road
when I was at Penland in 91 there was a guy there that I think his name was Judd Gerrard that was making air twist stemmed goblets solo , took him about 15 minutes and every move was precise. I'm not sure whatever happened to him. I had one of his goblets for a long time but may have gotten lost in a move.
Reply With Quote
  #11  
Old 10-18-2020, 12:19 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,050
Franklin Sankar is on a distinguished road
Bill said making the neck is the most important thing in making the piece.
That is so true.
Franklin
Reply With Quote
  #12  
Old 10-18-2020, 12:41 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,777
Eben Horton is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
Bill said making the neck is the most important thing in making the piece.
That is so true.
Franklin
I disagree. Not loosing the heat from your gather is the most important thing in goblet making. The jack line is important but you can still make a good goblet if your jack line is sub par.

Not so if you have to reheat a million times
__________________
<eben epoiese>
Reply With Quote
  #13  
Old 10-18-2020, 01:34 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,246
Greg Vriethoff is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
I disagree. Not loosing the heat from your gather is the most important thing in goblet making. The jack line is important but you can still make a good goblet if your jack line is sub par.

Not so if you have to reheat a million times
That's as far as I've ever gotten with a multi-part goblet. Get the foot open all nice and everything is straight, but I still let the moile get ice-cold. Never had a good transfer.

So I would have to agree that temperature is more important.

Everything we do in glass boils-down to temperature and time.
__________________
Temperature and time.
Reply With Quote
  #14  
Old 10-18-2020, 05:00 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,302
Pete VanderLaan is on a distinguished road
It also depends on the goblet you're making. Straight ahead goblets can be made in about seven minutes. If you want dragons flying out of cupids ass, it takes more time.
I really disliked making things that people were afraid to handle. Inevitably those things wound up high up and pushed back on shelves where they couldn't be damaged. When I was selling through Neiman Marcus, that was a frequent problem. The staff was terrified about damaging the work and they hated cleaning it. The buyers loved it. Onnce the work went in the direction of massive solid stuff, those problems went away.

Our house tender in NM managed to break the bulk of our stemware collection. Maria solved her own problems. My simple stems have lasted decades. The stems we sold in the Santa Fe gallery were usually thin but well executed. Chuck Savoie's stems did quite well though, an exception. The ones from Guy Corrie sold well . I never liked them since the lips were finished on a belt sander and that left a crunchy sort of feel in your mouth. I often felt the urge to bite them
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #15  
Old 10-18-2020, 05:48 PM
Ted Trower's Avatar
Ted Trower Ted Trower is online now
Registered User
 
Join Date: Apr 2002
Location: Ann Arbor, Michigan
Posts: 547
Ted Trower is on a distinguished road
Quote:
Originally Posted by Art Freas View Post
Our solo blower puts the granny next to it. When he picks up for incalmo he puts the blow pipe in the granny, picks up the cup with a punty and then takes them both back to the hole.
Sorry Art, but what's a "granny"
__________________
"It appears to me that glass men are the most given to drunkeness of any class of men I know" Peter Burt, recruiter in Europe, in a letter to Deming Jarves of the Boston and Sandwich glass company. -1826
Reply With Quote
  #16  
Old 10-18-2020, 06:50 PM
Jordan Kube Jordan Kube is offline
?
 
Join Date: Aug 2003
Location: Seattle, WA
Posts: 1,717
Jordan Kube is on a distinguished road
Pipe hanger
__________________
WWUD? Think for yourself.
Reply With Quote
  #17  
Old 10-19-2020, 03:54 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,050
Franklin Sankar is on a distinguished road
No hanging, I leave it on the bench and it does not sag if any at all. Does that mean not enough heat.?
Franklin
Reply With Quote
  #18  
Old 10-19-2020, 03:56 PM
Franklin Sankar's Avatar
Franklin Sankar Franklin Sankar is offline
Registered User
 
Join Date: Apr 2002
Location: Trinidad, West Indies
Posts: 4,050
Franklin Sankar is on a distinguished road
Granny. Old lady who is well respected. You don’t want to mess with her. She has a stick. Maybe that is what I need. One stick on my back and I will do it perfectly.
Franklin
Reply With Quote
  #19  
Old 10-19-2020, 04:40 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 696
Shawn Everette is on a distinguished road
Depends on your glass and what you're trying to do, but in many cases yes. Pretty much any studio I've worked in had a pipe hanger, doesn't need to be anything fancy.
Reply With Quote
  #20  
Old 10-19-2020, 04:54 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 723
Art Freas is on a distinguished road
Could not find a picture on line. Will take one next time I am down at the shop.
Reply With Quote
  #21  
Old 10-19-2020, 05:48 PM
Greg Vriethoff's Avatar
Greg Vriethoff Greg Vriethoff is offline
Registered User
 
Join Date: Jan 2007
Location: Charlotte, NC
Posts: 2,246
Greg Vriethoff is on a distinguished road
Quote:
Originally Posted by Franklin Sankar View Post
No hanging, I leave it on the bench and it does not sag if any at all. Does that mean not enough heat.?
Franklin
Technically, yes.

One of the "rules" my first glassblowing instructor (and subsequent ones as well) taught me is that the glass should always be moving. If your connections (jack line or punty) "freeze" it means the glass is too cold, and you're now going to have to put heat back into it before you try to crack it off (refer to Eben's comments above).

This is more challenging when blowing solo, and I have seen many people (myself included) get away with transfers that are far too cold. This is especially important when trying to work thinner. Thicker glass will "tolerate" more abuse at the bench, but will most often exact its revenge in the annealer.

Bill works very fast. If you watch his movements closely you will see that he does not leave the glass unattended for long. This is one of the downsides of the edited videos from CMOG. They are good for educating civilians, but if you can't watch someone working real-time you're going to miss a lot of important stuff.

Keep it hot and keep it turning is the mantra.
__________________
Temperature and time.
Reply With Quote
  #22  
Old 10-19-2020, 06:11 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,302
Pete VanderLaan is on a distinguished road
I count in my head from the beginning to the end. I know where I should be at any time. I don't talk at all. I don't hum, nothing.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #23  
Old 10-19-2020, 09:24 PM
Rich Samuel's Avatar
Rich Samuel Rich Samuel is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle, WA
Posts: 2,571
Rich Samuel is on a distinguished road
Does Pilchuck still ban pipe hangers in the name of teamwork only? Post-COVID, probably not a wise policy.
Reply With Quote
  #24  
Old 10-19-2020, 09:54 PM
Shawn Everette Shawn Everette is offline
Registered User
 
Join Date: Mar 2013
Location: Indianapolis, IN
Posts: 696
Shawn Everette is on a distinguished road
The last time I was on the pad about 12 years ago, I was probably 2 sheets to the wind doing a end of session solo challenge making a cowboy hat with only a modified copper pipe for a tool. I can't say as I remember seeing a pipe hanger, but it sure would have come in handy. Can't say as I remember much about the rest of the night either, and I might be better off for it.
Reply With Quote
  #25  
Old 10-19-2020, 10:02 PM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,777
Eben Horton is on a distinguished road
Back to goblets ..

Footed vases are a good warm up for making solo goblets. Look at English and Swedish ones for inspiration, as those styles of glass making are far more friendly to make and sell
__________________
<eben epoiese>
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 01:32 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.