Instant Batch Room

I though about building walls for a batch room and then remembered how cheap an 8' x 8' grow tent is these days. Nice thick walls, holes for vacuum or ventilation. I've got a Grizzley 2 stage HEPA cyclone dust extractor but I still have to figure out how to get the make up air just right. It sucks the walls of the tent in pretty good. It's actually working really well without it. Bulk chemicals on a pallet on the left, stainless table with shelving for colorants on the right. Mixer and floor scale along the back. I also have a dehumidifier that keeps the RH right at 35%.

This is really all the room you need to do it yourself. I've got space on the pallet for about 2000 pounds of bulk chemicals and the stainless table is perfect for everything else. I still have room for a trash can and small shop vac with HEPA filter. Best part is, I can roll it up and throw it in the garbage when I'm done.
Attached Images
File Type: jpg Batch room resize.jpg (49.9 KB, 72 views)
__________________
WWUD? Think for yourself.
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 10:55 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.