Metal in Aventurine

Quick question. In aventurine are these the right metals for the sparkles

Green-Chromium, Blue-Copper, Gold-Copper, Topaz-?, black-?

Has anyone figured a red aventurine?
Reply With Quote
  #2  
Old 08-24-2020, 08:34 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,167
Pete VanderLaan is on a distinguished road
If there are more than two true aventurines, I'm not aware of it.

Copper and chrome. Chrome Green and Copper brownish gold. Otherwise, there's mica introduced but they aren't the real deal. Chrome is far easier to make but a good aventurine will be achieved cooling the pot glass very slowly to room temp and then breaking up the chunks.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #3  
Old 08-24-2020, 09:01 AM
Eben Horton Eben Horton is offline
Registered User
 
Join Date: Apr 2002
Location: Wakefield, RI
Posts: 4,777
Eben Horton is on a distinguished road
I have only seen gold, dark green, light green and blue
__________________
<eben epoiese>
Reply With Quote
  #4  
Old 08-24-2020, 02:36 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,167
Pete VanderLaan is on a distinguished road
Quote:
Originally Posted by Eben Horton View Post
I have only seen gold, dark green, light green and blue
*****
Well, tradition says green and gold ( copper) but I can't see why cobalt, which is purely a saturation colorant couldn't color the chrome one some. They continue to be issues with expansion though.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #5  
Old 08-24-2020, 02:40 PM
Art Freas Art Freas is offline
Registered User
 
Join Date: Aug 2014
Location: Washington
Posts: 703
Art Freas is on a distinguished road
OCR sells blue but you have to use it carefully or you get cracking. Right on the edge of compatibility.
Reply With Quote
  #6  
Old 08-24-2020, 04:29 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 1,026
Larry Cazes is on a distinguished road
Are borosilicate aventurines true aventurines like their soft glass equivalents? 8 years ago I was attracted to boro for the color palette which seemed to have the best striking and sparkle glasses in a myriad of colors and I have not been disapointed.
Reply With Quote
  #7  
Old 08-24-2020, 06:27 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,167
Pete VanderLaan is on a distinguished road
I don't claim to know boro at all but at the same time, it would really have to be a batch glass to pull it off. You have to get inside the molecule.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #8  
Old 08-24-2020, 09:21 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 1,026
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
I don't claim to know boro at all but at the same time, it would really have to be a batch glass to pull it off. You have to get inside the molecule.
The variety of boro sparkles is huge both striking and not and the effects are stellar. Trautman made some of the best as well as a series of 3 different silver striking variants that are amazing.
Reply With Quote
  #9  
Old 08-25-2020, 09:17 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,167
Pete VanderLaan is on a distinguished road
The only stuff I ever tested for Paul was the 104 stuff after he had sold Northstar. One of his employees did take the class back in 2013. Smart guy.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #10  
Old 08-25-2020, 05:55 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 1,026
Larry Cazes is on a distinguished road
Quote:
Originally Posted by Pete VanderLaan View Post
The only stuff I ever tested for Paul was the 104 stuff after he had sold Northstar. One of his employees did take the class back in 2013. Smart guy.
Since then he reincorporated as TAG glass and now just recently resold the works to NS again. As TAG his glass was phenomenal.
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 06:18 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2020, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.