#51
|
||||
|
||||
The release can be measured in micrograms per hour and it goes up as the temperatures rise. Durk Valkema had some very convincing data on that over lead releases.
__________________
Where are we going and why am I in this basket? |
#52
|
|||
|
|||
So what is considered a high level of Borax. I was given a recipe with 2.3 % borax . Does anyone know what Spectrum's % is.What would be a good percent?
|
#53
|
||||
|
||||
Spectrum 2.0 has no borax . It was the SP 87 clone knock off. Sys96 was indeed high borax but none was what you might consider excessive. It's really more a question of what can't molecularly combine in the glass. So, it gasses off.
Cristalica would not appear to have a high borax content based on the formulation but they way it hits furnaces suggests otherwise. If you count molecules, which is the mole theory of glass, it presents a very different picture. Your furnace is the witness. Borax attacks fireclays and silicates. It's the yellow stain. It's your furnace dissolving.
__________________
Where are we going and why am I in this basket? |
#54
|
|||
|
|||
I can remember big yellow cakes all around th doors of the furnaces at RIT from the cullet. We used Gabbert 4C cullet. Man I hated that glass.
__________________
<eben epoiese> |
#55
|
|||
|
|||
cullet shortage
It seems here in this discussion that the only alternatives to cullet are to make your own batch or buy spruce pine. I have been melting glasma 705 batch since about 2006 that I buy from Bill Glasner. My melt temp is 2175f and I have really nice glass with no cords. Much better than any other glass I have used, optically, in my opinion. Although it is more expensive, (88 cent per lb.) I feel that I am saving a lot of money over spruce pine batch due to the lower energy cost and greatly increased furnace/crucible life. It is a perfect fit with spruce pine 87 and spectrum 2.0. It also cuts and polishes beautifully. I am using a Hugh Jenkins recuperated burner system in a really old pre-hub style furnace that John Chiles and I built in 1993 with an ifb liner.
|
#56
|
||||
|
||||
I think that's a nice glass but not for the inexperienced Sam. I have been told that it is a bit high on expansion by John Croucher but I've not measured it. I still think it would be very tough to melt in a wire furnace. It is brilliant stuff given the high barium content.
__________________
Where are we going and why am I in this basket? |
#57
|
|||
|
|||
It is no harder to melt than any other batch. It is just batch and maybe the inexperienced should stick with cullet? I don't really agree but that's ok. Get a decent respirator and a hepa filter vacuum and use both a lot.
And I don't have experience with anything other than gas furnaces. Last edited by Sam Stang; 02-04-2018 at 04:34 PM. |
#58
|
||||
|
||||
I don't think the upcoming dominance battle is going to be about batch. It will be cullet. Somewhere around 2000 the glass community switched from a body that melted a lot of different things to one which never melted anything but cullet/ It went to wire melters and all of the prior approaches were sort of dumped.
Theres nothing wrong with GLASMA at all. It;s a beautiful glass but if over fired has issues. That' s hardly the problem these days. If Bill wants to come on the board and hawk his product, that's fine. It's fine if Lewis does it as well. Tom pretty much never does. They probably all should stick their best foot forward. I don't have an agenda beyond dissemination of facts. The issue is more like what the middle of the road shop is going to do as they realize that Cristalica is not solving the problem, cuz it won't.
__________________
Where are we going and why am I in this basket? |
#59
|
|||
|
|||
What is in Glasma 705 that helps it melt at such a low temp?
__________________
<eben epoiese> |
#60
|
|||
|
|||
Hi Sam
What's your charging schedule like for the Glasma? I'm running a slightly different formula (702A) than the one that you get, but I'd be interested to compare. The instructions that I received from the UK supplier are: Raise furnace from working temp (2017F) to 2282F Top up crucible with batch, allow 30-40 minutes between charges Maintain furnace at 2282F for five hours after last charge Ramp down to working temperature, but allow 1.5-2 hours before working I include a squeeze down to 1900F and work at a slightly hotter temperature (2050F), but otherwise it works pretty well. If you're loading at a colder temperature, are you raising it up for the fining part of the cycle? Or holder it longer at the lower temperature? Scott |
#61
|
|||
|
|||
Hi Scott,
I charge at a really low temp over the weekend. maybe 1920 or so. My burner is really under powered so heat recovery takes a while. Down to the mid 1800's after a few scoops each time. I have it full by Sunday night and leave it at a setting that will slowly climb up to 2000 by Monday morning and then I heat it up to 2175 (over 5 hours or so) and cook it for 3 hours at that temperature. My turndown is also a really slow curve due to the heat recuperation. I haven't carefully tracked it but it seems to be staying above 2100 for a couple more hours at least. So, the furnace is hot for a long time. Eventually squeezing just below 1900 by mid day Monday. Work at 1900 to 1950. I make a lot of murrini pieces gathering over very soft colors so I want it cold. I have a 2nd small furnace (hub mu800) with 2.0 cullet or color that I use on Mondays and charge it while blowing glasma or if it is not on, I can just make cane stuff or I work in my machine shop. Btw, I am getting 3 years out of a crucible. About 150 lb pot. |
#62
|
|||
|
|||
Thanks, Sam, that's interesting to hear and that's a very impressive pot life. I'm in a situation where I often have to do overnight charges, so the higher temps allow me to go through the process more quickly. No second furnace to take up the slack, either.
Why is the proto-Hub furnace underpowered? Wasn't John using the Eclipse Thermjet burners back then? |
#63
|
||||
|
||||
Given that charge cycle, the pot should last quite a long while. It seems quite cold to me. I'm charging now and pretty much run it up to 2250F before I start. Keep in mind that all of these issues undergo quite a change when there's no flue and that is the case with most wire melters which in turn makes the glass formation a real issue.
__________________
Where are we going and why am I in this basket? |
#64
|
|||
|
|||
Hey Scott,
The electricity would go out a lot in my rural area so I wanted to run it without a blower. I used a Gib tip venturi for many years. I started melting it at 2225 and gradually dropped the temp bit by bit without noticing any decrease in glass quality. |
#65
|
|||
|
|||
Quote:
Hello Pete, and hello to everyone, As Pete knows me, but the others in the thread might not, I must mention that I work for Cristalica and handle the sales worldwide, so I can get some direct info about the current situation. 😊 What Pete explains about production capacity was absolutely true for that past period of time when he knew of our furnace directly. At this point, I also want to thank him for introducing us to the US market and the vast array of clients we are now happy to supply, via either Spruce Pine, or Olympic Color Rods. I want to give an update to that, i.e. that since Pete and us have spoken directly, the larger furnace in Germany has been fired up to meet demand. During the past year, in parallel with Spectrum not producing any more, we have noticed a higher demand and this being said, we want to also take the opportunity and inform you of an increased production capacity (which we will gradually keep raising) and a renewed guarantee that our capacities are planned long-term so as to ensure that our Premium product is accessible and available to all the artists we admire. As such, we want to ensure you – our existing and possible future clients – that we will meet the demand for glass without problems, as we have planned. About the borax issue, as Pete mentioned, we have discussed this at that point in time. As in Europe and in other parts of the world, this issue has never arisen before, we are now again looking into what we can specifically do for clients encountering this problem. Please kindly forward any such photos, questions and description of this to our direct distributors, Olympic Color Rods and Spruce Pine, so we get word of any questions you may have and see further steps in this respect together with our partners on the US market. We hope you do enjoy working with our cullet and look forward to seeing you all in la bella Italia, at the GAS Conference in Murano! Glass is magic. Andreea Virag |
#66
|
||||
|
||||
Andreea,
I sent you an email.
__________________
Where are we going and why am I in this basket? |
#67
|
|||
|
|||
The volatilisation of boron introduced by the addition of Borax, from glass at temperatures of 1100 C and above is substantial due to its vapor pressure.
As an example in E-glass 10 – 25% boron loss is calculated, water vapor has significant impact on the evaporation of boron. Boron volatiles condensate between 400 – 800 C and form all sorts of borates along the way playing havoc with alumna silicate refractory. |
#68
|
||||
|
||||
Thanks Durk. So I would imagine that 10 mole borax has a greater impact than five mole would?
__________________
Where are we going and why am I in this basket? |
#69
|
|||
|
|||
The evaporation rates depend on the process conditions in the glass furnace, like:
Glass melt composition (at the surface); Temperature of the glass melt surface; Composition of the atmosphere. Especially the water vapor (air-fuel versus oxy- fuel) and the carbon monoxide contents just above the melt are important. In furnace atmospheres with high water vapor mainly meta-boric acid is released. Exposure time of a glass melt volume to the combustion atmosphere and Local gas velocities and turbulence intensity just above the glass melt surface. Electric melting has an advantage here but in a flue-less furnace the gathering port gets the full load. In alkali melts, NaBO2 and KBO2 will evaporate. In melts where CaF2 is added as flux boron seems to be released as OBF |
#70
|
||||
|
||||
The main destructive activity I see with it is in the gathering port or forehearth and the door. It makes a tar baby like material that has real staying power. Those furnace parts over here are largely insulating castables in the doors and some other 35% alumina refractories going up to 60%. But the silicates and fireclays certainly get consumed. I'm not seeing it in the crucibles- yet but the incorrect assumption that an electric unit did not need a flue was simply dead wrong using these materials. The little wire melters get it the worst. You just can't use any fluorine in electrics. It's either nitrate or lithium driven and lithium is pricey stuff. I did unsuccessfully try to get Dobern to get the stuff out of the glass 18 months ago but I was not surprised to see them pass on changing it. It seems to me right now that if Oceanside were to decide to make the purloined SP87 cullet in Tijuana that it would really cripple the popularity of the Cristalica which is a shotgun marriage right now. . The down side? They'd have to do it right. Life without borax would be better. I do wonder where the price will settle. No one is making any money at $1.00 lb.
__________________
Where are we going and why am I in this basket? |
#71
|
|||
|
|||
I would take your class on making clear glass.
|
#72
|
|||
|
|||
Heather, I would get a copy of the 4th edition of Glass Notes. Pete wrote an excellent section in there about mixing your own glass. Next, the color making sub-forum here on Craftweb has some posts that are real gems of information. A little more time consuming is searching through the whole site for information but is also very rewarding. The glass notes thing is probably the closest thing there is to an instruction manual. Dave Bross has posted what looks to be a couple of nice clear formulas as a place to start. Expect to pay at least $3000 for the equipment and chemicals to get you started. I think I am paying $.55 a pound for the clear base I am using in the quantities I am buying in. Just as a spitball estimate I would add $.25 per pound in your labor to measure and mix.
__________________
WWUD? Think for yourself. |
#73
|
|||
|
|||
Thanks, Jordan. Much obliged for the advice. I won't wait on Pete to have a class.
Are you melting your clear in that slick wire melter? |
#74
|
||||
|
||||
Indeed I have no rescue classes in my plans today. I don't find clear to be very hard. My costs on making it are higher than the ones Jordan cites but not all clears use the same stuff. I did lay out some very straight ahead 96 clears for Henry in Glassnotes IV but now the book itself has gotten quite pricey and it's not to say that I haven't moved to new places in the last ten years. 3K may be about right for the cap outlay, I suspect a bit less. Under a dollar a lb for clear is doable. Wire melters are not a good place to start.
Spruce Pine mixes my formula for me now- nice to the old man. I may go back to doing it myself but materials in rural areas is now an issue. I think the thing that discourages me the most in todays glass community is how frail the response is to being self starters. Dust, poisons, it can all be dealt with easily. At one time, we were adventurers, not so much now. As Henry said "Glass is fragile". That's true. It's not guaranteed either.
__________________
Where are we going and why am I in this basket? |
#75
|
|||
|
|||
I'm melting exclusively color in the wire melter although I'm not sure how slick it is. I have some improvements I'd like to make. Got me up and running pretty quick though.
__________________