Thumbs up rewettable canvas

I don't know what dip lag is.
I use "rewettable canvas" over the frax on furnace tops and other places. It is woven with some powdery refractory stuff, and is worked with a scissors and spray bottle. It covers, sticks to itself, forms, and protects. Dries like shoe leather. Used a lot in asbestos containment. Call an asbestos abatement place. It is something like 50 inches wide and sold by the yard. Works great for containing frax fibres. Hope this helps.
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off
Forum Jump


All times are GMT -5. The time now is 12:45 AM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
© CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.