Moly cooling

A friend sent me a schematic of a European built Moly furnace. At that time we were changing a pot and doing some upgrades on one of our furnaces. I noticed that the cooling tubes on the schematic seemed to be metal and quite a lot larger than what we do here. It made for a nice uncluttered look.

It made me start thinking about this area and I decided to build a plenum with some 2" flexible tailpipe attached to it. This would allow us to aim the air flow at the element tops. I gathered up some parts and formulated a plan.Then I had to leave town.

When I got back my plans had been modified and my guys had come with a new and I think better approach. We installed one of these a few months ago and it seems to be working well. We did the second one last week and that's what these photos are about. Still a work in progress but I like how it's going.
The blower is from Grainger and costs I think $112. It puts out 463 CFM. If you stand at the edge of the furnace and look at the elements you can feel a nice little breeze on your face.
Attached Images
File Type: jpg P7290033-6.jpg (36.1 KB, 246 views)
File Type: jpg P7290003-1.jpg (38.6 KB, 234 views)
File Type: jpg P7290005-5.jpg (47.3 KB, 211 views)
File Type: jpg P8020052-3.jpg (43.7 KB, 221 views)
File Type: jpg P8020053-2.jpg (43.5 KB, 229 views)
Reply With Quote
  #2  
Old 08-03-2010, 11:33 AM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,738
Steve Stadelman is on a distinguished road
That is a really nice way to do that Rollin.
__________________
If all you wanted to do was express yourself artistically, you should have obtained a field watercolor set and a pad of acid-free paper. You chose a media with INFRASTRUCTURE baby!
Reply With Quote
  #3  
Old 08-03-2010, 12:14 PM
Rollin Karg Rollin Karg is offline
Registered User
 
Join Date: Apr 2002
Location: Kechi, KS
Posts: 924
Rollin Karg is on a distinguished road
Thanks boss !!
Reply With Quote
  #4  
Old 08-03-2010, 12:48 PM
Larry Cazes Larry Cazes is offline
Registered User
 
Join Date: Feb 2006
Location: San Jose, CA
Posts: 1,020
Larry Cazes is on a distinguished road
Nice manifold, Rollin. Very clean design.
Reply With Quote
  #5  
Old 08-03-2010, 02:10 PM
Charles Friedman Charles Friedman is offline
Registered User
 
Join Date: Apr 2002
Location: Seattle Wa
Posts: 600
Charles Friedman is on a distinguished road
Paint it all gray. It will help it disappear.
That seams like a bit too large of a blower.
But, if it works? it works.
__________________
"Glass will save the world from ourselfs" CharlesF
Reply With Quote
  #6  
Old 08-03-2010, 02:48 PM
Rollin Karg Rollin Karg is offline
Registered User
 
Join Date: Apr 2002
Location: Kechi, KS
Posts: 924
Rollin Karg is on a distinguished road
Quote:
Originally Posted by Charles Friedman View Post
That seams like a bit too large of a blower.
Yeah ,probably. I just took a guess at the size to start and at $112 I can't see I would saving much to downsize. I do think some reflective paint would be a good idea.
Reply With Quote
  #7  
Old 08-03-2010, 05:35 PM
Kenny Pieper Kenny Pieper is offline
Registered User
 
Join Date: Feb 2003
Location: Burnsville N.C.
Posts: 844
Kenny Pieper is on a distinguished road
Rollin I am curious. Have you found that Steve's way with the two washers welded to a tube that blows the air just on the top shaft of the element to be inadequate?
Reply With Quote
  #8  
Old 08-03-2010, 06:15 PM
Rollin Karg Rollin Karg is offline
Registered User
 
Join Date: Apr 2002
Location: Kechi, KS
Posts: 924
Rollin Karg is on a distinguished road
Eben, the way it's setup, all the air is directed at the top of the elements and I can't see it having much impact on the overall temp of the furnace. The European unit had the airflow coming down from the top and I think that might have a small impact.

Kenny, I'm getting more air where I want it and I don't have hoses to deal with, so this what I like about it. The other way works, but I think this is a little better. We're using four furnaces right now and that's a lot of hoses. Plus with this system the top of the element is a little less cluttered. I don't see this an earth shaking improvment, but I think it's a little better.
Reply With Quote
  #9  
Old 08-03-2010, 10:16 PM
Scott Garrelts
Guest
 
Posts: n/a
looks like it should be a lot easier to change out a broken element. :crossing fingers:

plastic hoses melt, sheet metal usually doesnt.

i like it
Reply With Quote
  #10  
Old 08-04-2010, 12:00 AM
Steve Stadelman Steve Stadelman is offline
Registered User
 
Join Date: Jun 2002
Location: Portland oregon area
Posts: 3,738
Steve Stadelman is on a distinguished road
I think that this is a really good way to do this, i started using hoses because I got it out of the kanthal super handbook. There are lots of ways to skin a cat and keeping the transition from the strap to the heater is what is important.
__________________
If all you wanted to do was express yourself artistically, you should have obtained a field watercolor set and a pad of acid-free paper. You chose a media with INFRASTRUCTURE baby!
Reply With Quote
  #11  
Old 08-04-2010, 06:17 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,274
Pete VanderLaan is on a distinguished road
It does look good. I would again stress that cooling the leads at your transformer is a place where you can prevent a lot of serious damage. I have a blower running there whenever I go to High Fire.
__________________
Where are we going and why am I in this basket?
Reply With Quote
  #12  
Old 08-04-2010, 06:22 PM
Paul Hayworth Paul Hayworth is offline
Registered User
 
Join Date: Jun 2002
Location: Port Macquarie
Posts: 153
Paul Hayworth is on a distinguished road
steel flex piping for cold air

http://www.gsl.cz/en/products/pot-furnaces.html
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On
Forum Jump


All times are GMT -5. The time now is 02:41 PM.


All published comments within these message boards are the opinions of its contributor and does not represent
the opinion(s) of the owner(s) of this website. Please see the Terms of Use file for more details.

Books to Help Artists Avoid Online Scams: Top 10 Email Scams | Social Media Scams

Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2021, Jelsoft Enterprises Ltd.
CraftWEB.com. Opportunity Network. 2008. All Rights Reserved.